Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric

Category Polymer , Thermoset , Epoxy , Epoxy/Glass SMC
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.516 MPa
800.0 psi
Flatwise tensile, RT
310 MPa

@Temperature 71.0 °C
45000 psi

@Temperature 160 °F
1/2 hr
400 MPa

@Temperature 23.0 °C
58000 psi

@Temperature 73.4 °F
Tensile Modulus 20.7 GPa

@Temperature 71.0 °C
3000 ksi

@Temperature 160 °F
1/2 hr
22.1 GPa

@Temperature 23.0 °C
3210 ksi

@Temperature 73.4 °F
Flexural Yield Strength 0.896 MPa
130 psi
Long beam flexure, RT
448 MPa

@Temperature 71.0 °C
65000 psi

@Temperature 160 °F
1/2 hr
538 MPa

@Temperature 23.0 °C
78000 psi

@Temperature 73.4 °F
Flexural Modulus 20.7 GPa

@Temperature 71.0 °C
3000 ksi

@Temperature 160 °F
1/2 hr
22.1 GPa

@Temperature 23.0 °C
3210 ksi

@Temperature 73.4 °F
Compressive Yield Strength 310 MPa

@Temperature 71.0 °C
45000 psi

@Temperature 160 °F
1/2 hr
483 MPa

@Temperature 23.0 °C
70100 psi

@Temperature 73.4 °F
Compressive Modulus 22.1 GPa

@Temperature 71.0 °C
3210 ksi

@Temperature 160 °F
1/2 hr
23.4 GPa

@Temperature 23.0 °C
3390 ksi

@Temperature 73.4 °F
Shear Strength 29.0 MPa

@Temperature 23.0 °C
4210 psi

@Temperature 73.4 °F