Material Notes:
Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 330 MPa

@Temperature 177 °C
47900 psi

@Temperature 351 °F
438 MPa

@Temperature 24.0 °C
63500 psi

@Temperature 75.2 °F
Tensile Modulus 24.4 GPa

@Temperature 177 °C
3540 ksi

@Temperature 351 °F
27.7 GPa

@Temperature 24.0 °C
4020 ksi

@Temperature 75.2 °F
Compressive Yield Strength 270 MPa

@Temperature 177 °C
39200 psi

@Temperature 351 °F
469 MPa

@Temperature 24.0 °C
68000 psi

@Temperature 75.2 °F
Compressive Modulus 22.1 GPa

@Temperature 177 °C
3210 ksi

@Temperature 351 °F
30.1 GPa

@Temperature 24.0 °C
4370 ksi

@Temperature 75.2 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.029
Laminate
Dry Resin Content (%) 34-40
Prepreg
Fiber Volume (%) 41.2
Laminate
Flow (%) 15-25