Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 22.1 GPa @Temperature 93.3 °C |
3200 ksi @Temperature 200 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-722 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-722 is a modified 350°F cure epoxy system with excellent processing characteristics for vacuum bag, press, and autoclave molding.Key Features and Benefits:Epoxy resin system optimized f.. |
|||
Compressive Modulus | 22.1 GPa @Temperature -53.9 °C |
3200 ksi @Temperature -65.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 22.1 GPa @Temperature 21.1 °C |
3200 ksi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Compressive Modulus | 22.1 GPa @Temperature 23.9 °C |
3200 ksi @Temperature 75.0 °F |
Dry; 8HS form; ASTM D695 |
Park Electrochemical Nelcote® F-555 Phenolic Prepreg, C2 Reinforced Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shiel.. |
|||
Compressive Modulus | 22.1 GPa @Temperature 177 °C |
3210 ksi @Temperature 351 °F |
|
Hexcel® F161 Epoxy Resin, 7781 Glass Fabric Hexcel designation: 7781-38"-F161; Fiber: 75-1/0Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 93.0 °C |
3210 ksi @Temperature 199 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 181 Glass Fabric Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 24.0 °C |
3210 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, 220 Glass Fabric Information provided by HexCel |
|||
Compressive Modulus | 22.1 GPa @Temperature 71.0 °C |
3210 ksi @Temperature 160 °F |
1/2 hr |
Hexcel® HexPly® F515 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F515; Fiber 150-1/2Information provided by HexCel |