Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Strength = 8700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 60.0 MPa

@Strain 2 %
8700 psi

@Strain 2 %
ISO 604
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data)
Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, ..
Compressive Strength 60.0 MPa

@Strain 2 %
8700 psi

@Strain 2 %
ISO 604
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data)
Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX..
Compressive Strength 60.0 MPa

@Temperature 200 °C
8700 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
Compressive Strength 60.0 MPa

@Temperature 250 °C
8700 psi

@Temperature 482 °F
ISO 604
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, ..
Compressive Strength 60.0 MPa

@Temperature 200 °C
8700 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant..
Compressive Strength 60.0 - 70.0 MPa

@Temperature 100 °C
8700 - 10200 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 127 S Dense Refractory Castable
Description: Curon 127 S castable is characterized by a very high strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks: These value..
Compressive Strength 60.0 - 70.0 MPa

@Temperature 100 °C
8700 - 10200 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 160 H SiC (R) Dense Self Flowing Refractory Castable
Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resis..
Compressive Strength 60.0 - 70.0 MPa

@Temperature 100 °C
8700 - 10200 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 13 SC Dense Refractory Castable
Description: Curon 13 SC is a spinel based castable with a very low silica content and therefore it is suitable for direct contact with all kinds of aluminum/alloys and fluxes in aluminum melting/ho..
Compressive Strength 60.0 MPa

@Temperature 1000 °C
8700 psi

@Temperature 1830 °F
Cold Crushing
Sharadaa Ceramics VELECRETE RC 101 Rodding Castables
Description: The Rodding Castables offered by us are user friendly in nature and does not require high energy mixing machines and vibrators. Free flowing in nature, these castables are designed in c..