Material Notes:
Description: Flucon 160 H SiC (R) is a self-flowing low cement castable, characterized by a high strength and good slag resistance. Because of the presence of SiC this material has a very good resistance to several aggressive slags. This material is especially developed for application in the steel industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.55 - 2.65 g/cc
0.0921 - 0.0957 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 60.0 - 70.0 MPa

@Temperature 100 °C
8700 - 10200 psi

@Temperature 212 °F
Cold Crushing Strength
190 - 210 MPa

@Temperature 1400 °C
27600 - 30500 psi

@Temperature 2550 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.15 - 1.35 W/m-K

@Temperature 100 °C
7.98 - 9.37 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.18 - 1.38 W/m-K

@Temperature 600 °C
8.19 - 9.58 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.29 - 1.49 W/m-K

@Temperature 1400 °C
8.95 - 10.3 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1650 °C
3000 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1400 °C
-0.200 - 0.200 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 66 %
66 %
Fe2O3 1.0 %
1.0 %
SiC 7.0 %
7.0 %
SiO2 25 %
25 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2550 kg
Mixing Water 6-7 liters
per 100 kgs dry material