Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 19.0 MPa @Strain 5 % |
2760 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Compressive Strength | 19.0 MPa @Strain 2 % |
2760 psi @Strain 2 % |
ISO 604 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Compressive Strength | 19.0 MPa @Strain 5 % |
2760 psi @Strain 5 % |
ISO 604 |
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data) FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application.. |
|||
Compressive Strength | 19.0 MPa @Strain 5 % |
2760 psi @Strain 5 % |
ISO 604 |
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data) TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance |
|||
Compressive Strength | 19.0 MPa @Temperature 90.0 °C |
2760 psi @Temperature 194 °F |
|
Pyrotek Pyrocast SC-2600 Castable Refractory Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes .. |
|||
Compressive Strength | 19.0 MPa @Temperature 1370 °C |
2760 psi @Temperature 2500 °F |
|
Pyrotek Pyrocast SC-2600 Castable Refractory Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes .. |