Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Mica Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Fluorosint®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties High maximum allowable service temperature in air (260°C continuously) Excellent chemical and hydrolysis resistance Outstanding UV- and weather resistance Physiologically inert (suitable for food contact, except Fluorosint 500, Fluorosint MT-01) Inherent low flammability Good electrical insulating properties
Physical Properties Metric English Comments
Density 2.32 g/cc
0.0838 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium <= 0.10 %
<= 0.10 %
50% RH
Water Absorption at Saturation 1.5 - 2.5 %
1.5 - 2.5 %
Mechanical Properties Metric English Comments
Hardness, Rockwell R 55
55
ISO 2039-2
Hardness, Shore D 65
65
Ball Indentation Hardness 60.0 MPa
8700 psi
ISO 2039-1
Tensile Strength 7.00 MPa
1020 psi
at Yield; ISO 527-1/-2
Elongation at Break 15 %
15 %
ISO 527-1/-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-1/-2
Tensile Modulus 1.75 GPa
254 ksi
ISO 527-1/-2
Flexural Strength 13.0 MPa
1890 psi
Compressive Strength 12.0 MPa

@Strain 1 %
1740 psi

@Strain 1 %
ISO 604
19.0 MPa

@Strain 2 %
2760 psi

@Strain 2 %
ISO 604
25.0 MPa

@Strain 5 %
3630 psi

@Strain 5 %
ISO 604
K Factor (ISO) 12 µm/km
12 µm/km
Charpy Impact Unnotched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.20 - 0.30
0.20 - 0.30
Limiting Pressure Velocity 0.250 MPa-m/sec
7140 psi-ft/min
at 1 m/s unlubricated
0.400 MPa-m/sec
11400 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 23.0 - 100 °C
27.8 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.770 W/m-K
5.34 BTU-in/hr-ft²-°F
Melting Point 327 °C
621 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 260 °C
500 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index >= 95 %
>= 95 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+13 ohm-cm
>= 1.0e+13 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Strength 11.0 kV/mm
279 kV/in
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Acceptable
Acceptable
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable