Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Quadrant Engineering Plastics Products
Trade Name Borotron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very suitable for slowing down fast neutrons to lower energy thermal (slow) neutrons, which are then absorbed by the added boron compound. Whereas both PE-HMW and PE-UHMW are suitable for neutron shielding, PE-UHMW is often preferred because of its better deformation behaviour at high temperatures and its superior impact strength and wear resistance Effectively attenuates neutron radiation particles and minimises the gamma radiation released during their capture Very good wear and abrasion resistance High impact strength (particularly PE-UHMW) Excellent chemical resistance Low coefficient of friction Very low water absorption Moderate mechanical strength, stiffness and creep resistance Excellent machinability
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ISO 1183-1
Outgassing - Total Mass Loss 0.14 %
0.14 %
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
Ball Indentation Hardness 35.0 MPa
5080 psi
ISO 2039-1
Tensile Strength 17.0 MPa
2470 psi
at Yield; ISO 527-1/-2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/-2
Elongation at Yield 18 %
18 %
ISO 527-1/-2
Tensile Modulus 0.875 GPa
127 ksi
ISO 527-1/-2
Flexural Strength 17.0 MPa
2470 psi
Compressive Strength 8.00 MPa

@Strain 1 %
1160 psi

@Strain 1 %
ISO 604
12.5 MPa

@Strain 2 %
1810 psi

@Strain 2 %
ISO 604
19.0 MPa

@Strain 5 %
2760 psi

@Strain 5 %
ISO 604
K Factor (ISO) 14 µm/km
14 µm/km
Charpy Impact Unnotched NB
NB
ISO 179-1/1eU
Charpy Impact, Notched 4.00 J/cm²
19.0 ft-lb/in²
Partial Break; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.30
0.15 - 0.30
Sand Slurry 140
140
Limiting Pressure Velocity 0.0500 MPa-m/sec
1430 psi-ft/min
at 1 m/s unlubricated
0.0800 MPa-m/sec
2280 psi-ft/min
at 0.1 m/s unlubricated
Thermal Properties Metric English Comments
CTE, linear 185 µm/m-°C

@Temperature 23.0 - 100 °C
103 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.650 W/m-K
4.51 BTU-in/hr-ft²-°F
Melting Point 135 °C
275 °F
DSC, 10°C/min.; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C
108 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
Oxygen Index <= 20 %
<= 20 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+12 ohm
>= 1.0e+12 ohm
IEC 60093
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Acceptable
Acceptable
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Acceptable
Alkalies, Weak Acceptable
Acceptable
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Unacceptable
Unacceptable
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Limited
Limited
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable