Mechanical Properties Metric English Comments
Compressive Strength 19.0 MPa

@Strain 5 %
2760 psi

@Strain 5 %
ISO 604
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data)
Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su..
Compressive Strength 19.0 MPa

@Strain 2 %
2760 psi

@Strain 2 %
ISO 604
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Compressive Strength 19.0 MPa

@Strain 5 %
2760 psi

@Strain 5 %
ISO 604
Quadrant EPP Fluorosint® HPV PTFE + additives, bearing grade, compression moulded (ISO Data)
FDA compliant Fluorosint HPV is a high performance Fluorosint bearing grade, optimized for high pressure-velocity capabilities and very low wear. Fluorosint HPV was developed for bearing application..
Compressive Strength 19.0 MPa

@Strain 5 %
2760 psi

@Strain 5 %
ISO 604
Quadrant EPP TIVAR® 1000 EC PE-UHMW + specific additives (ISO Data)
TIVAR 1000 EC is a PE-UHMW grade containing specific additives rendering this material a lower surface resistivity than TIVAR 1000 antistatic, improving electrical conductivity and UV-resistance
Compressive Strength 19.0 MPa

@Temperature 90.0 °C
2760 psi

@Temperature 194 °F
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes ..
Compressive Strength 19.0 MPa

@Temperature 1370 °C
2760 psi

@Temperature 2500 °F
Pyrotek Pyrocast SC-2600 Castable Refractory
Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes ..