Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pyrotek Pyrocast SC-2600 Castable Refractory

Category Ceramic , Carbide
Manufacturer Pyrotek, Inc.
Trade Name Pyrocast
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pyrotek Pyrocast SC-2600 Castable Refractory.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pyrocast SC-2600 is a high purity silicon carbide based refractory for applications requiring high thermal conductivity, resistance to metal and flame abrasion.ApplicationsFilter boxes Burner tubes Troughs Tap out blocks Special refractory shapes Baffles Filter bowl tiles AdvantagesResistant to metal Resistant to flame abrasion High thermal conductivity Withstands high temperatures Extremely hard Information provided by Pyrotek.
Physical Properties Metric English Comments
Density 2.40 g/cc
0.0867 lb/in³
Mechanical Properties Metric English Comments
Modulus of Rupture 0.00800 GPa

@Temperature 90.0 °C
1.16 ksi

@Temperature 194 °F
0.0220 GPa

@Temperature 815 °C
3.19 ksi

@Temperature 1500 °F
0.0300 GPa

@Temperature 1370 °C
4.35 ksi

@Temperature 2500 °F
Compressive Strength 10.0 MPa

@Temperature 815 °C
1450 psi

@Temperature 1500 °F
19.0 MPa

@Temperature 90.0 °C
2760 psi

@Temperature 194 °F
19.0 MPa

@Temperature 1370 °C
2760 psi

@Temperature 2500 °F
Thermal Properties Metric English Comments
Thermal Conductivity 9.40 - 10.8 W/m-K
65.2 - 75.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1480 °C
2700 °F
Shrinkage -0.600 %

@Temperature 1300 °C
-0.600 %

@Temperature 2370 °F
Linear
Component Elements Properties Metric English Comments
Al2O3 12 %
12 %
CaO 3.0 %
3.0 %
Other 1.0 %
1.0 %
SiC 83 %
83 %
SiO2 1.0 %
1.0 %
Users viewing this material also viewed the following: