Gouda Vuurvast CURON 100 Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 100 Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modifications are available on demand.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 1.85 - 1.95 g/cc
0.0668 - 0.0704 lb/in³
After drying at 110°C
Particle Size <= 4000 µm
<= 4000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 10.0 - 20.0 MPa

@Temperature 815 °C
1450 - 2900 psi

@Temperature 1500 °F
Cold Crushing Strength
25.0 - 35.0 MPa

@Temperature 100 °C
3630 - 5080 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.450 - 0.550 W/m-K

@Temperature 100 °C
3.12 - 3.82 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.530 - 0.630 W/m-K

@Temperature 600 °C
3.68 - 4.37 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.550 - 0.650 W/m-K

@Temperature 815 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Shrinkage -0.200 - 0.200 %

@Temperature 815 °C
-0.200 - 0.200 %

@Temperature 1500 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 25 %
25 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 1850 kg
Mixing Water 16-20 liters
per 100 kgs dry material