Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 10.0 - 20.0 MPa @Temperature 1300 °C |
1450 - 2900 psi @Temperature 2370 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 145 F Sp Dense Refractory Castable Description: Curon 145F Special is a very fine graded castable and can be applied for the casting of complicated shapes.Remarks: These values apply to cast products. Also available in gunning variet.. |
|||
Compressive Strength | 10.0 - 20.0 MPa @Temperature 815 °C |
1450 - 2900 psi @Temperature 1500 °F |
Cold Crushing Strength |
Gouda Vuurvast CURON 100 Dense Refractory Castable Description: Curon 100 is a general purpose castable for temperatures up to 1000°C.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM". Other modification.. |