Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.60 GPa @Temperature 23.0 °C |
522 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 3.60 GPa @Temperature 90.0 °C |
522 ksi @Temperature 194 °F |
|
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Mineral filler. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good therm.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 120 °C |
522 ksi @Temperature 248 °F |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 90.0 °C |
522 ksi @Temperature 194 °F |
|
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Tensile Modulus | 3.60 GPa @Temperature 150 °C |
522 ksi @Temperature 302 °F |
|
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa & Middle East; Asia Pacific; Europe; Latin.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 120 °C |
522 ksi @Temperature 248 °F |
|
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Toughened. Glass fibers. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 120 °C |
522 ksi @Temperature 248 °F |
|
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 60.0 °C |
522 ksi @Temperature 140 °F |
|
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 60.0 °C |
522 ksi @Temperature 140 °F |
|
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Tensile Modulus | 3.60 GPa @Temperature 120 °C |
522 ksi @Temperature 248 °F |
|
LATI Latamid 6 CUVHPX10 G/35 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. High viscosity. Toughened. Glass fibers. Heat stabilized. UV stabilized. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 150 °C |
522 ksi @Temperature 302 °F |
|
LATI Latamid 6 H2 G/30-V0AF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Tensile Modulus | 3.60 GPa @Temperature 90.0 °C |
522 ksi @Temperature 194 °F |
|
LATI Latamid 6 H2 G/30-V2HF PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. UL94 V-2 classified, halogens-based flame retardants and red phosphorous freeAvailability: Africa & Middle East; Asia Pacific; Europe.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 150 °C |
522 ksi @Temperature 302 °F |
|
LATI Latamid 66 H2 G/25 PA 66, 25% Glass Fiber Reinforced, Heat Stabilized Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termop.. |
|||
Tensile Modulus | 3.60 GPa @Temperature 23.0 °C |
522 ksi @Temperature 73.4 °F |
|
LATI Latan 13 S/30 POM, 30% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |