Polymer Property : Seal Strength = 200 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Seal Strength >= 200 g/25 mm
>= 200 g/in
at 135°C, 15 psi pressure and 1 sec.
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor - Low catalyst residuals in FINA 7450HC result in improved color stability.Clarity/Impact - The random copolymer structure of FINA 7450HC improves its ..
Seal Strength >= 200 g/25 mm
>= 200 g/in
at 135°C, 15 psi pressure and 1 sec.
Total PPR 8573 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m..
Seal Strength >= 200 g/25 mm
>= 200 g/in
at 135°C, 15 psi pressure and 1 sec.
Total PPR 8473 Polypropylene, Film Extrusion Grade
Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very ..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
LPS, 0.5 sec, Both Sides; ExxonMobl Method
ExxonMobil Bicor™ 21MBT621 OPP Film
Product Description: Biaxially oriented transparent polypropylene film with heat sealable coating applied to both side. The static resistant feature of this film prevents the attraction of dust, and..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 105 °C
200 g/in

@Pressure 0.500 psi,
Temperature 221 °F
LSP, 0.5 sec; ExxonMobil Method
ExxonMobil Bicor™ 25MBT666 OPP Film
Product Description: Biaxially oriented polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping offering unique aspect and cost reduction advant..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
0.5 sec; ExxonMobil Method
ExxonMobil Bicor™ 30MB666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
LPS, 0.5 sec; ExxonMobil Method
ExxonMobil Bicor™ 30MBT666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. This film is specifically suitable for unsupported overwrapping, offering unique aspect and cost r..
Seal Strength 200 g/25 mm

@Pressure 0.00345 MPa,
Temperature 100 °C
200 g/in

@Pressure 0.500 psi,
Temperature 212 °F
0.5 sec, Untreated Surface; ExxonMobl Method
ExxonMobil Bicor™ 20MBT666 OPP Film
Product Description: Bicor 20MBT666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. This film is specifically suitable for unprinted overwrapping, offering unique as..
Seal Strength 200 - 410 g/25 mm
200 - 410 g/in
Average value: 231 g/25 mm Grade Count:10
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Seal Strength 200 - 810 g/25 mm

@Temperature 80.0 - 140 °C
200 - 810 g/in

@Temperature 176 - 284 °F
Average value: 419 g/25 mm Grade Count:65
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Seal Strength 200 - 810 g/25 mm

@Pressure 0.00345 - 0.276 MPa
200 - 810 g/in

@Pressure 0.500 - 40.0 psi
Average value: 419 g/25 mm Grade Count:65
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..