Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 200 - 810 g/25 mm @Temperature 80.0 - 140 °C |
200 - 810 g/in @Temperature 176 - 284 °F |
Average value: 419 g/25 mm Grade Count:65 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Seal Strength | 200 - 810 g/25 mm @Pressure 0.00345 - 0.276 MPa |
200 - 810 g/in @Pressure 0.500 - 40.0 psi |
Average value: 419 g/25 mm Grade Count:65 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |