Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Seal Strength = 810 g/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Seal Strength 200 - 810 g/25 mm

@Temperature 80.0 - 140 °C
200 - 810 g/in

@Temperature 176 - 284 °F
Average value: 419 g/25 mm Grade Count:65
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Seal Strength 200 - 810 g/25 mm

@Pressure 0.00345 - 0.276 MPa
200 - 810 g/in

@Pressure 0.500 - 40.0 psi
Average value: 419 g/25 mm Grade Count:65
Overview of materials for Polypropylene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr..
Copyright © lookpolymers.com All Rights Reserved