Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 200 - 410 g/25 mm | 200 - 410 g/in | Average value: 231 g/25 mm Grade Count:10 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |