Mechanical Properties Metric English Comments
Flexural Yield Strength 47.0 MPa
6820 psi
ISO METHOD 178
NYCOA 567 PA 6
plasticized general purpose molding and extrusion grade used in shoe heels and mono.Information provided by NYCOA, Inc.
Flexural Yield Strength 47.0 MPa
6820 psi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East)
High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Yield Strength 47.0 MPa
6820 psi
ASTM D790
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade
Data provided by North Wood Plastics, Inc.
Flexural Yield Strength 47.0 MPa
6820 psi
Solvay Specialty Polymers Halar® 300 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Flexural Yield Strength 47.0 MPa
6820 psi
Solvay Specialty Polymers Halar® 500 ECTFE Fluoropolymer  (discontinued **)
Data provided by the manufacturer.HALAR® Fluoropolymers have excellent barrier properties, high resistance to a variety of corrosive chemicals and solvents, low flammability, and ease of processing..
Flexural Yield Strength 47.0 MPa
6820 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ML004S PP
LNP* LUBRICOMP* ML004S is a compound based on Polypropylene resin containing 20% PTFE. Added features of this material include: Wear Resistant, Heat Stabilized.
Flexural Yield Strength 47.0 - 210 MPa
6820 - 30500 psi
Average value: 153 MPa Grade Count:43
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..