Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 121 - 210 MPa | 17500 - 30500 psi | Average value: 161 MPa Grade Count:18 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Flexural Yield Strength | 32.0 - 210 MPa | 4640 - 30500 psi | Average value: 117 MPa Grade Count:217 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Flexural Yield Strength | 47.0 - 210 MPa | 6820 - 30500 psi | Average value: 153 MPa Grade Count:43 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |