Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 100 - 269 MPa | 14500 - 39000 psi | Average value: 141 MPa Grade Count:10 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Flexural Yield Strength | 132 - 269 MPa | 19100 - 39000 psi | Average value: 209 MPa Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Flexural Yield Strength | 68.0 - 269 MPa | 9860 - 39000 psi | Average value: 157 MPa Grade Count:16 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |