Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 55.0 - 240 MPa | 7980 - 34800 psi | Average value: 92.9 MPa Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Yield Strength | 140 - 240 MPa | 20300 - 34800 psi | Average value: 182 MPa Grade Count:6 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 120 - 240 MPa | 17400 - 34800 psi | Average value: 189 MPa Grade Count:6 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Flexural Yield Strength | 40.7 - 240 MPa | 5900 - 34800 psi | Average value: 112 MPa Grade Count:28 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Flexural Yield Strength | 45.0 - 240 MPa @Temperature -40.0 - 90.0 °C |
6530 - 34800 psi @Temperature -40.0 - 194 °F |
Average value: 116 MPa Grade Count:4 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |