Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min; ASTM D790 |
Ovation Polymers RIGITRON 10030 GF Polycarbonate, 30% Glass Reinforced PC - Glass reinforced (30 %), high tensile strength, stiffness and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared accor.. |
|||
Flexural Yield Strength | 140 - 240 MPa | 20300 - 34800 psi | Average value: 182 MPa Grade Count:6 |
Overview of materials for Phenolic, Resole, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8232G HS 25% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8232G HS is a heat stabilized, 25% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. Its resista.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem DH1004F PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM HU1004 PEI High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM 1110 PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East) Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. Noryl GFN1520V cust spec 1977 has been certified for potable water applications up to 85C in Europe and No.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ISO 178 |
Hexcel® HexPly® M18 356°F (180°C) Curing Epoxy Matrix HexPly® M18 has been developed to fulfill the requirements of the aerospace industry for primary structures using standard manufacturing processes. The matrix has improved properties which allow ea.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM D790 |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Flexural Yield Strength | 140 - 180 MPa | 20300 - 26100 psi | ASTM D790 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 140 - 180 MPa | 20300 - 26100 psi | ASTM D790 |
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | ASTM Data |
BASF Capron® 8260 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 is a 40% mineral reinforced polyamide 6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability includi.. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Flexural Yield Strength | 140 MPa | 20300 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |