Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 13.8 - 131 MPa | 2000 - 19000 psi | Average value: 75.1 MPa Grade Count:28 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Yield Strength | 13.8 - 193 MPa | 2000 - 28000 psi | Average value: 130 MPa Grade Count:68 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Flexural Yield Strength | 13.8 - 48.3 MPa | 2000 - 7000 psi | Average value: 29.2 MPa Grade Count:22 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Flexural Yield Strength | 13.8 - 1150 MPa | 2000 - 167000 psi | Average value: 254 MPa Grade Count:71 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi.. |
|||
Flexural Yield Strength | 13.8 - 250 MPa | 2000 - 36300 psi | Average value: 142 MPa Grade Count:122 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |