Polymer Property : Flexural Yield Strength = 250 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 103 - 250 MPa
15000 - 36300 psi
Average value: 172 MPa Grade Count:47
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi..
Flexural Yield Strength 133 - 250 MPa
19300 - 36300 psi
Average value: 194 MPa Grade Count:11
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Flexural Yield Strength 109 - 250 MPa
15800 - 36300 psi
Average value: 180 MPa Grade Count:45
Overview of materials for Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 40% Glass Fiber Filled". Specific grades with glass content between 35% an..
Flexural Yield Strength 158 - 250 MPa
22900 - 36300 psi
Average value: 192 MPa Grade Count:14
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Flexural Yield Strength 75.0 - 250 MPa
10900 - 36300 psi
Average value: 141 MPa Grade Count:63
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
Flexural Yield Strength 50.0 - 250 MPa
7250 - 36300 psi
Average value: 117 MPa Grade Count:50
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Flexural Yield Strength 13.8 - 250 MPa
2000 - 36300 psi
Average value: 142 MPa Grade Count:122
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..