Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Compounding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake EMAC® SP2242 Specialty Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. For use as heat seal layer, adhesive layer, or modifier for cost/performance enhancement. They are soft, pliable and tough at ambient and freezing temperatures and exhibit excellent ESCR. These polymers exhibit high solids fillability and compatibility with a wide range of polymers. This facilitates their uses as bases for all-purpose concentrates for addition to a wide spectrum of polymers. They process like LDPE.Applications/UsesFilmsEastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.
Physical Properties Metric English Comments
Base Resin Density 0.939 g/cc
0.0339 lb/in³
ASTM D1505
Methyl Acrylate Content 17.5 %
17.5 %
Thickness 38.1 microns
1.50 mil
ASTM D374
Base Resin Melt Index 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D638
Film Elongation at Break, MD 365 %
365 %
ASTM D882
Film Elongation at Break, TD 695 %
695 %
ASTM D882
Elongation at Break 770 %
770 %
500mm/min; ASTM D638
Secant Modulus, MD 0.0560 GPa
8.12 ksi
0.01; ASTM D882
Secant Modulus, TD 0.0560 GPa
8.12 ksi
0.01; ASTM D882
Elmendorf Tear Strength, MD 1.15 g/micron
29.2 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 4.99 g/micron
127 g/mil
ASTM D1922
Dart Drop 6.04 g/micron
153 g/mil
ASTM D1709A
Film Tensile Strength at Break, MD 19.0 MPa
2760 psi
ASTM D882
Film Tensile Strength at Break, TD 14.0 MPa
2030 psi
ASTM D882
Heat Seal Strength Initiation Temperature 70.0 °C
158 °F
Eastman
Thermal Properties Metric English Comments
Melting Point 84.0 °C
183 °F
DSC
Brittleness Temperature <= -73.0 °C
<= -99.4 °F
ASTM D746
Optical Properties Metric English Comments
Haze 49 %
49 %
ASTM D1003
Gloss 15 %
15 %
ASTM D2457