Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elmendorf Tear Strength, MD | 7.09 g/micron | 180 g/mil | ASTM D1922 |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | ISO 6383-2 |
Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high o.. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | ISO 6383-2 |
Total LLDPE LL 1810 Linear Low Density Polyethylene - Blown Film LL 1810 is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 can be processed at high outpu.. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | ASTM D1922 |
Total Lotrene® Q1018N Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | ASTM D1922 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Elmendorf Tear Strength, MD | 7.09 g/micron | 180 g/mil | ASTM D1922 |
ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications Product Description: Exact 3027 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3027 is designed for both monolayer and multilayer coe.. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | |
Dow AFFINITY™ FM 1570 Polyolefin Plastomer AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and .. |
|||
Elmendorf Tear Strength, MD | 7.10 g/micron | 180 g/mil | |
Dow AFFINITY™ PL 1845 Polyolefin Plastomer Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical. |
|||
Elmendorf Tear Strength, MD | 7.09 g/micron | 180 g/mil | ASTM D1922 |
ExxonMobil LL 3201.22 Premium High Strength Film Resin
(discontinued **) LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow.. |