Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer Total Atofina
Trade Name LLDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total LLDPE LL 1810 H Linear Low Density Polyethylene - Blown Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LL 1810 H is an ethylene-butene copolymer produced in a gas phase reactor. It is designed for delivering competitive performance in most blown film applications.LL 1810 H can be processed at high output rates with moderate extrusion pressure, good bubble stability and gauge control on blown film machine designed for LLDPE.LL 1810 H can advantageously be blended with LDPE or other PE resins used in blown film mono extrusion or coextrusion to improve film properties.LL 1810 H is suited for many applications in the field of consumer, industrial, food or hygiene packaging such as collation shrink, liners, Form-Fill-Seal, heavy-duty sacks, refuse sacks or other bags and non-packaging applications like agriculture films e.g. tunnel and mulching films.Contains antioxidant, slip agent and antiblock agent.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.921 g/cc
0.921 g/cc
ISO 1183
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Antiblock Level 3200 ppm
3200 ppm
Slip Level 1500 ppm
1500 ppm
Erucamide
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 11.0 MPa
1600 psi
ISO 527-3
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 527-3
Film Elongation at Break, MD 800 %
800 %
ISO 527-3
Film Elongation at Break, TD 850 %
850 %
ISO 527-3
Elmendorf Tear Strength, MD 7.10 g/micron
180 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 12.2 g/micron
310 g/mil
ISO 6383-2
Dart Drop Test 150 g
0.331 lb
ISO 7765-1
Film Tensile Strength at Break, MD 38.0 MPa
5510 psi
ISO 527-3
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ISO 527-3
1% Secant Modulus, MD 215 MPa
31200 psi
ISO 178
1% Secant Modulus, TD 245 MPa
35500 psi
ISO 178
Thermal Properties Metric English Comments
Melting Point 122 °C
252 °F
ISO 11357
Vicat Softening Point 100 °C
212 °F
ISO 306
Optical Properties Metric English Comments
Haze 12 %
12 %
ISO 14782
Gloss 57 %
57 %
at 45°; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 180 - 220 °C
356 - 428 °F
Extrusion Temp
Die Opening >= 0.180 cm
>= 0.0709 in
Blow-up Ratio (BUR) 2.0 - 3.0
2.0 - 3.0