Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Film Grade , Polyethylene (PE)
Manufacturer Exxon Chemical
Trade Name EXACT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Exact 3027 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3027 is designed for both monolayer and multilayer coextruded cast film applicatiosn requiring excellent toughness and heat sealing performance. Typical applicatiosn include seal layers for meat, poultry, and cheese packaging, lamination films, heavy duty bags, and cereal box liner packaging. Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesApplications:Cast FilmHeavy Duty BagsLamination Film Data provided by the manufacturer, Exxon Chemical.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Exxon Method
Thickness 20.3 microns
0.800 mil
Melt Flow 3.5 g/10 min
3.5 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 6.27 MPa
909 psi
ASTM D882
Film Tensile Strength at Yield, TD 4.30 MPa
624 psi
ASTM D882
Film Elongation at Break, MD 490 %
490 %
ASTM D882
Film Elongation at Break, TD 810 %
810 %
ASTM D882
Film Elongation at Yield, MD 10 %
10 %
ASTM D882
Film Elongation at Yield, TD 8.0 %
8.0 %
ASTM D882
Secant Modulus, MD 0.0669 GPa
9.70 ksi
1% secant; ASTM D882
Secant Modulus, TD 0.0758 GPa
11.0 ksi
1% secant; ASTM D882
Puncture Energy 6.44 J
4.75 ft-lb
Exxon Method
Elmendorf Tear Strength, MD 7.09 g/micron
180 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 9.84 g/micron
250 g/mil
ASTM D1922
Dart Drop 9.06 g/micron
230 g/mil
ASTM D1709
Film Tensile Strength at Break, MD 58.0 MPa
8410 psi
ASTM D882
Film Tensile Strength at Break, TD 35.0 MPa
5080 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point 90.0 °C
194 °F
Exxon Method
Optical Properties Metric English Comments
Haze 0.40 %
0.40 %
ASTM D1003
Gloss 94 %
94 %
45°; ASTM D-2457
Descriptive Properties Value Comments
Puncture Force 14 lbf
Exxon Method
Users viewing this material also viewed the following: