Mechanical Properties Metric English Comments
Shear Modulus 3.00 - 5.00 GPa
435 - 725 ksi
Average value: 3.83 GPa Grade Count:3
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Shear Modulus 3.00 - 5.82 GPa
435 - 844 ksi
Average value: 3.73 GPa Grade Count:14
Overview of materials for Phenolic, Novolac, Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values..
Shear Modulus 3.00 GPa
435 ksi
Calculated
Plenco 4485 Phenolic, Granular, Injection Molded
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is a..
Shear Modulus 3.00 GPa
435 ksi
Calculated
Plenco 7100 Phenolic, Nodular, Injection Molded
PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit..
Shear Modulus 3.00 GPa
435 ksi
In-Plane, RT, Dry; EN6031
Hexcel® HexPly® M42 180°C (350°F) Curing Epoxy Matrix, 54%/G1088 Glass/Carbon Fiber
Information provided by HexCel
Shear Modulus 3.00 GPa
435 ksi
Calculated
Plenco 7307 Phenolic, Granular, Transfer Molded
PLENCO 07307 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties. Type ASTM 5948 CFG, and UL recognized under component file E40654. 07307 is a..