Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 4485 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 4485 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 04485 is a mineral filled phenolic molding compound offering excellent heat resistance, electrical resistance, and dimensional stability. UL recognized under component file E40654. 04485 is available in black, brown, and red.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.640 g/cc
0.0231 lb/in³
ASTM D1895
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Water Absorption 0.212 %
0.212 %
ASTM D570
Linear Mold Shrinkage 0.0081 cm/cm
0.0081 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 84
84
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 0.82 %
0.82 %
ASTM D638
Tensile Modulus 8.10 GPa
1170 ksi
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 7.50 GPa
1090 ksi
ASTM D790
Compressive Strength 195 MPa
28300 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 3.00 GPa
435 ksi
Calculated
Izod Impact, Notched 0.151 J/cm
0.283 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.172 J/cm²
0.819 ft-lb/in²
ASTM D256
Impact 96
96
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 40.0 - 130 °C
27.8 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 166 °C
331 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
Oxygen Index 31 %
31 %
ASTM D2863
Shrinkage 0.29 %
0.29 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+11 ohm-cm
1.90e+11 ohm-cm
ASTM D247
Dielectric Constant 5.3
5.3
ASTM D150
Dielectric Strength 10.0 kV/mm
254 kV/in
Short Time; ASTM D149
Dissipation Factor 0.056
0.056
ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638