Mechanical Properties Metric English Comments
Shear Modulus 3.00 - 5.00 GPa
435 - 725 ksi
Average value: 3.83 GPa Grade Count:3
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Shear Modulus 4.60 - 5.00 GPa
667 - 725 ksi
Average value: 4.73 GPa Grade Count:3
Overview of materials for Nylon 6, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E..