Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 3.00 - 5.00 GPa | 435 - 725 ksi | Average value: 3.83 GPa Grade Count:3 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Shear Modulus | 4.60 - 5.00 GPa | 667 - 725 ksi | Average value: 4.73 GPa Grade Count:3 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |