Plenco 7100 Phenolic, Nodular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Flock Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7100 Phenolic, Nodular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourability. UL recognized under component file E40654. 07100 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.55 %
0.55 %
ASTM D570
Linear Mold Shrinkage 0.0085 cm/cm
0.0085 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 78
78
ASTM D785
Tensile Strength, Ultimate 52.0 MPa
7540 psi
ASTM D638
Elongation at Break 0.79 %
0.79 %
ASTM D638
Tensile Modulus 7.80 GPa
1130 ksi
ASTM D638
Flexural Strength 72.0 MPa
10400 psi
ASTM D790
Flexural Modulus 6.40 GPa
928 ksi
ASTM D790
Compressive Strength 182 MPa
26400 psi
ASTM D695
Poissons Ratio 0.30
0.30
ASTM D638
Shear Modulus 3.00 GPa
435 ksi
Calculated
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.227 J/cm²
1.08 ft-lb/in²
ASTM D256
Impact 193
193
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.3 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.400 W/m-K

@Temperature 100 °C
2.78 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 183 °C
361 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Oxygen Index 27.1 %
27.1 %
ASTM D2863
Shrinkage 0.39 %
0.39 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 6.60e+11 ohm-cm
6.60e+11 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 9.70 kV/mm
246 kV/in
Short Time; ASTM D149
Dissipation Factor 0.055
0.055
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638