PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PolyOne Corporation
Trade Name LubriOne™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne LubriOne™ PS-30GF/15T Natural Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.64 g/cc
1.64 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 103 MPa
14900 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 6.89 GPa
999 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 165 MPa
23900 psi
1.3 mm/min; ASTM D790
Flexural Modulus 6.89 GPa
999 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.800 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Coefficient of Friction, Dynamic 0.57
0.57
vs. Steel - Dynamic; ASTM D1894
Coefficient of Friction, Static 0.41
0.41
vs. Steel - Static; ASTM D1894
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 216 °C

@Thickness 6.35 mm
421 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Features Good Chemical Resistance
High Heat Resistance
High Rigidity
Lubricated
Semi Crystalline
Forms Pellets
Generic Material PBT
Generic Name Polybutylene Terephthalate (PBT)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliance Components
Automotive Applications
Bearings
Business Equipment
Consumer Applications
Conveyor Parts
Gears
Industrial Applications
Printer Parts
Pulleys
Rollers
Copyright © lookpolymers.com All Rights Reserved