Material Notes:
LNP* Stat-loy* AF306 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber. Added features of this material include: Antistat.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
1.29 g/cc
0.0466 lb/in³
ASTM D792
Moisture Absorption 3.00 %
3.00 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0045 cm/cm

@Time 86400 sec
0.0045 in/in

@Time 24.0 hour
ISO 294
0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ASTM D638
43.0 MPa
6240 psi
ISO 527
Tensile Strength, Yield 38.0 MPa
5510 psi
ASTM D638
43.0 MPa
6240 psi
ISO 527
Elongation at Break 1.0 %
1.0 %
ASTM D638
1.0 %
1.0 %
ISO 527
Elongation at Yield 1.0 %
1.0 %
ASTM D638
1.1 %
1.1 %
ISO 527
Tensile Modulus 6.01 GPa
872 ksi
1 mm/min; ISO 527
6.89 GPa
999 ksi
50 mm/min; ASTM D638
Flexural Strength 48.0 MPa
6960 psi
ASTM D790
63.0 MPa
9140 psi
ISO 178
Flexural Modulus 5.51 GPa
799 ksi
ASTM D790
5.70 GPa
827 ksi
ISO 178
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.50 J/cm
4.68 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J
4.43 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 113 µm/m-°C

@Temperature -40.0 - 40.0 °C
62.8 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
114 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
43.2 µm/m-°C

@Temperature -40.0 - 40.0 °C
24.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C
160 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
95.0 °C

@Thickness 3.20 mm
203 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
ASTM D257