Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 218 V30 Black 21 N PA66, 30% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyamide PA66/6, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific and EuropeProduct Applications: TECHNYL® B 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry; especially for the production of unpainted external parts due to its excellent surface finish, such as: door mirror housing, door handles. This product is available in grey and black.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ISO 527 Type 1A
Elongation at Break 8.0 %
8.0 %
ISO 527 Type 1A
Tensile Modulus 6.50 GPa
943 ksi
ISO 527 Type 1A
Flexural Modulus 4.70 GPa
682 ksi
ISO 178
Izod Impact, Notched (ISO) 19.0 kJ/m²
9.04 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 9.20 J/cm²
43.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+11 ohm-cm
1.50e+11 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %