Mechanical Properties Metric English Comments
Tensile Modulus 3.38 GPa
490 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
Tensile Modulus 3.38 GPa
490 ksi
ASTM D638
Plaskolite Optix® DA Digital Acrylic Sheet
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup..
Tensile Modulus 3.38 GPa
490 ksi
0.2 in/min; 0.050" thickness; ASTM D-638
Chevron Phillips EA3350 Crystal Polystyrene  (discontinued **)
High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni..
Tensile Modulus 3.38 GPa
490 ksi
ASTM D638
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Tensile Modulus 3.38 GPa
490 ksi
50 mm/min; ISO 527-2/50; ASTM D638
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding ..
Tensile Modulus 3.38 GPa
490 ksi
ISO 527-2/50; ASTM D638
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin
Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL..
Tensile Modulus 3.38 GPa
490 ksi
0.2 in/min; 0.050" thickness; ASTM D-638
Chevron Phillips EA3025 Crystal Polystyrene  (discontinued **)
High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar..
Tensile Modulus 3.38 GPa
490 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled  (discontinued **)
Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation.