Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.38 GPa | 490 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | ASTM D638 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | 0.2 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | ASTM D638 |
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | 50 mm/min; ISO 527-2/50; ASTM D638 |
Styron CALIBREâ„¢ 5101-15 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resin is 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding .. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | ISO 527-2/50; ASTM D638 |
Styron CALIBREâ„¢ 5101-8 Polycarbonate Resin Overview: CALIBREâ„¢ 5101 Polycarbonate resins 10% glass-reinforced and provides increased modulus and improved heat distortion resistance with minimal shrinkage. This resin offers outstanding UL.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | 0.2 in/min; 0.050" thickness; ASTM D-638 |
Chevron Phillips EA3025 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar.. |
|||
Tensile Modulus | 3.38 GPa | 490 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AT-30GB/000 Acetal-Copolymer, Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledInformation provided by PolyOne Corporation. |