Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
Quadrant EPP Nylatron® GS Nylon, Extruded MoS2 Filled Type 66 (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
Quantum PPS Information provided by Quantum Advanced Engineering Plastics |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled
(discontinue Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA 6/10 (Asia Pacific) LNP* Lubricomp* QAP22S is a compound based on Nylon 6/10 resin containing PTFE, Aramid Fiber, Silicone. Added features of this material include: Internally Lubricated, Heat Stabilized. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP QAP22S PA6.10 LNP* LUBRICOMP* QAP22S is a compound based on Nylon 6/10 resin containing 10% PTFE/Silicone, 10% Aramid Fiber. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Stat-kon RX89129 PA 66 LNP* Stat-Kon RX89129 is a compound based on Nylon 6,6. Fillers are proprietary.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | |
Master Bond EP45HTMED Epoxy Resists Radiation and Steam Sterilization Description: Master Bond Polymer System EP45HTMED is a two component heat cured epoxy system for high performance structural bonding, sealing, coating and casting. It is especially designed for the .. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
Ensinger TECATRON™ PPS Polyphenylene sulfide (PPS) TECATRON PPS is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves TECATRON.. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM Data |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM Data |
Dow Tyril® 1000B SAN TYRIL® 1000B SAN copolymer offers the best balance of physical properties of all TYRIL grades. It also provides excellent processability and chemical resistance, superior heat resistance, and good .. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
Asahi Kasei Thermylene® P6-20FG-1740 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
Tensile Modulus | 3.31 GPa @Temperature 80.0 °C |
480 ksi @Temperature 176 °F |
ISO Data |
BASF Ultramid® SEGM35 H1 BK-126 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid SEGM35 H1 BK-126 is a 40% glass/mineral reinforced injection molding grade. It offers enhanced surface appearance, it also exhibits similar UV weathering characteristics compared to 8267G .. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
LNP Lubricomp® IBL-4416 Polyamide 6/12 Copolymer, Glass Bead Reinforced, Silicone Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | ASTM D638 |
Ensinger ENSIFIDE® PPS (Polyphenylene Sulfide) - Extruded Products
(discontinued **) ENSIFIDE is a high performance thermoplastic that combines good mechanical properties with excellent thermal and chemical resistance properties. There is no known solvent that dissolves ENSIFIDE at.. |
|||
Tensile Modulus | 3.31 GPa | 480 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON MFD03 PP (Asia Pacific) LNP* Stat-kon* MFD03 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |