Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled  (discontinue

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-10GF/000 FR Acrylonitrile Butadiene Styrene (ABS), Glass/Carbon Fiber Filled  (discontinue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass/Carbon Fiber ReinforcedIgnition ResistantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.286 g/cc
1.286 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hr. Immersion, -; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.9 MPa
5500 psi
Type 1 - Rigids, Break, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.31 GPa
480 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 37.9 MPa
5500 psi
ASTM D790
Flexural Modulus 3.31 GPa
480 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
All Colors, 0.125 in thick; UL 94
Processing Properties Metric English Comments
Melt Temperature 210 - 238 °C
410 - 460 °F
Molding
Mold Temperature 54.4 - 65.6 °C
130 - 150 °F
Drying Temperature 65.6 °C
150 °F
2 hrs