Axiall 9190 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9190 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9190 was developed to aid compliance with source reduction initiatives especially when low temperature impact strength is a concern. It has superior properties, which in most cases will facilitate light weighting of the package. This product is used for a variety of opaque packaging applications including toiletries, household chemicals, automotive care products and charcoal lighter fluid.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.02 MPa
6385 psi
ASTM D-638
Tensile Modulus 2.99 GPa
434 ksi
ASTM D-638
Flexural Strength 73.43 MPa
10650 psi
ASTM D-790
Izod Impact, Notched 6.83 J/cm

@Thickness 6.35 mm,
Temperature 0.000 °C
12.8 ft-lb/in

@Thickness 0.250 in,
Temperature 32.0 °F
ASTM D-256
8.60 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
16.1 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
10.9 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
20.5 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
13.4 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
25.1 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 229 kJ/m²
109 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 61.22 °C
142.2 °F
ASTM D-648
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1305
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 31.5