SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl PKN4736 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
NORYL PKN4736 is a PPO+HIPS extrusion grade for dilution with polystyrene resin. It is suitable for (microwavable) food packaging and is compliant with US and European food contact regulations.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 59.0 MPa
8560 psi
50 mm/min; ISO 527
Elongation at Break 14 %
14 %
50 mm/min; ISO 527
Tensile Modulus 2.65 GPa
384 ksi
1 mm/min; ISO 527
Flexural Yield Strength 95.0 MPa
13800 psi
2 mm/min; ISO 178
Flexural Modulus 2.35 GPa
341 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature -30.0 °C
5.23 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
16.0 kJ/m²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.80 J/cm²

@Temperature 23.0 °C
8.57 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 124 °C
255 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 152 °C
306 °F
Rate A/50; ISO 306