Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 17.2 GPa | 2490 ksi | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent creep .. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Dry) Amodel® AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater tha.. |
|||
Tensile Modulus | 17.2 GPa @Temperature 100 °C |
2490 ksi @Temperature 212 °F |
4; ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | 5 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® A-1145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® A-1145 HS is a 45% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, very high flexural modulus and very high tensile strength. Excellent cr.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 23570 Phenolic, Compression Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 23570 Phenolic, Injection Grade Durez 23570 Black Phenolic is a glass and mineral filled two-stage, special purpose molding material. It is designed for high strength, good dimensional stability, and electrical properties even aft.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32245 Phenolic, Compression Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Sumitomo Bakelite Durez® 32245 Phenolic, Injection Grade Durez 32245 Black Phenolic is a two-stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stabilit.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM-D790 |
Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | 5.0 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | Conditioned; ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1145 HS is a 45% glass reinforced heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0... |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | ASTM-D790 |
Polyram Polytron A50N02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Tensile Modulus | 17.2 GPa | 2490 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Tensile Modulus | 17.2 GPa @Temperature 100 °C |
2490 ksi @Temperature 212 °F |
ISO 527-2 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically .. |