EMS-Grivory Grivory® BG-50 FC PA6-GF50

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BG-50 FC PA6-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surface finishEasy flowingEasy processing Application examples are stressed functional parts for applications such as swing bars for packing containers and bath seats in the sanitary field.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.58 g/cc
0.0571 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 155 MPa
22500 psi
conditioned; ISO 527-1/-2
240 MPa
34800 psi
dry; ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
dry; ISO 527-1/-2
6.0 %
6.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
17.2 GPa
2490 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
dry; ISO 179/1eU
9.50 J/cm²
45.2 ft-lb/in²
conditioned; ISO 179/1eU
8.50 J/cm²

@Temperature 30.0 °C
40.4 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
9.00 J/cm²

@Temperature 30.0 °C
42.8 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
dry; ISO 179/1eA
2.50 J/cm²
11.9 ft-lb/in²
conditioned; ISO 179/1eA
1.10 J/cm²

@Temperature 30.0 °C
5.23 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.20 J/cm²

@Temperature 30.0 °C
5.71 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
200 °C
392 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 180 °C
356 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Descriptive Properties Value Comments
Automotive Interior
Powertrain and Chassis
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Product Attributes Improved flowability and demoulding