Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.0 °C |
2390 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber
(discontinued **) PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® K-FHG0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-50 PA6-GF50 Product description: Grilon BG-50 is a heat stabilized, normal viscosity PA6 injection molding grade with 50% glass fibers. Grilon BG-50 has the following important properties: High stiffnessGood su.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1 |
Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade (PBT+X)-GF45Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Arnite® TV4 491 (PBT+PET)-GF50 |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |