Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER A9045 PBT, 45% glass fiber reinforced, improved surface quality, reduced warpage, food grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
(PBT+X)-GF45Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
similar to ISO 62 test
Melt Flow 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ISO 527-1
Elongation at Break 2.0 %
2.0 %
ISO 527-1
Tensile Modulus 16.5 GPa
2390 ksi
ISO 527-1
Charpy Impact Unnotched 6.50 J/cm²
30.9 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 1.10 J/cm²
5.23 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
UL Registered; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type (PBT+X)-GF45
Users viewing this material also viewed the following: