Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 50% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, Dry As Molded &.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high tensile strength, high flexural modulus, low warpage, excellent dimensional stability, and low moisture absorption. This grade was designed specifically to be cost effective when high stiffness, good dimensional stability, and superior electrical properties are required. With a comparative tracking index of 450 volts and a deflection temperature of 505°F (263°C), this resin is a potential thermoset replacement in many electrical applications. Potential applications for AMODEL AF-1550 V0 resin include electrical relays, housings, motor starters, contactors, circuit breakers, and terminal blocks. This grade of AMODEL resin can also withstand the demanding vapor phase and infrared reflow soldering processes commonly used in the electronics industry for connectors and devices requiring surface mount technology.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material conditioned at 50% RH.
Physical Properties Metric English Comments
Density 1.82 g/cc
0.0658 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM E831
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
0.0030 in/in
ASTM E831
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 145 MPa
21000 psi
ASTM D638
Elongation at Break 1.3 %
1.3 %
ASTM D638
Tensile Modulus 16.5 GPa
2390 ksi
ASTM D638
Flexural Yield Strength 214 MPa
31000 psi
ASTM D790
Flexural Modulus 14.1 GPa
2050 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.86 J/cm
7.23 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 310 °C
590 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 263 °C
505 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.00e+15 ohm-cm
4.00e+15 ohm-cm
ASTM D257
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
ASTM D257
Dielectric Constant 4.3

@Frequency 100 Hz
4.3

@Frequency 100 Hz
ASTM D150
4.3

@Frequency 1e+6 Hz
4.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 25.8 kV/mm
655 kV/in
ASTM D149
Dissipation Factor 0.0050

@Frequency 100 Hz
0.0050

@Frequency 100 Hz
ASTM D150
0.012

@Frequency 1e+6 Hz
0.012

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance >= 300 sec
>= 300 sec
UL 746A
Comparative Tracking Index 450 V
450 V
Hot Wire Ignition, HWI >= 150 sec
>= 150 sec
High Amp Arc Ignition, HAI 69 arcs

@Thickness 0.800 mm
69 arcs

@Thickness 0.0315 in
High Voltage Arc-Tracking Rate, HVTR 4.00 mm/min
0.157 in/min
Processing Properties Metric English Comments
Melt Temperature 321 - 338 °C
610 - 640 °F
Injection