Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Arnite® TV4 491 (PBT+PET)-GF50

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET Blend, Glass Filled
Manufacturer DSM Engineering Plastics
Trade Name Arnite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Arnite® TV4 491 (PBT+PET)-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.72 g/cc
0.0621 lb/in³
ISO 1183
Water Absorption 0.30 %
0.30 %
Sim. To ISO 62
Moisture Absorption 0.150 %
0.150 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 165 MPa
23900 psi
ISO 527-1/-2
Elongation at Break 1.8 %
1.8 %
ISO 527-1/-2
Tensile Modulus 16.5 GPa
2390 ksi
ISO 527-1/-2
Charpy Impact Unnotched 5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Users viewing this material also viewed the following: