Material Notes:
CapabilitiesGauge: .005’ to .025” (126 to 635µm)Width: 12” to 62” (305 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coating available5 strategic manufacturing locationsPropertiesRemarkable clarityExcellent stiffness to allow downgaugingSuperb yieldEasily thermoformedFDA compliant to CFR 21 #177.1640Kosher MaterialInformation provided by Alcoa Kama Co.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Thickness 127 - 635 microns
5.00 - 25.0 mil
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 - 41.4 MPa
4000 - 6000 psi
ASTM D638
Elongation at Break 20 - 60 %
20 - 60 %
ASTM D638
Tensile Modulus 2.07 - 2.41 GPa
300 - 350 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Processing Temperature 132 - 154 °C
270 - 310 °F
Thermoforming Temp
Descriptive Properties Value Comments
Resistance to Acid Good to Excellent
Resistance to Alcohols Good to Excellent
Resistance to Alkalis Excellent
Resistance to Fat, Grease, and Oil Good
Resistance to Hydrocarbon Solvents Poor
Resistance to Strong Oxidizers Poor
Yield, in²/lb/mil 26360