Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron Magnum™ 4435 ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Styron
Trade Name Magnum™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Magnum™ 4435 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.THE MAGNUM 4400 series of ignition resistant ABS resins are specifically engineered for information and technology equipment applications. These resins can be injection molded or extruded into applications like monitors, copiers and printers; housings and surge protectors.MAGNUM 4435 ABS resin is ignition resistant with excellent processability and practical toughness.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM Data
Melt Density 1.10 g/cc
0.0397 lb/in³
Melt density
Linear Mold Shrinkage 0.0055 cm/cm
0.0055 in/in
Melt Flow 11 g/10 min

@Load 3.80 kg,
Temperature 230 °C
11 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 30.3 MPa
4390 psi
ASTM Data
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM Data
Elongation at Break 35 %
35 %
ASTM Data
Tensile Modulus 2.07 GPa
300 ksi
ASTM Data
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM Data
Impact Test 32.0 J

@Temperature 23.0 °C
23.6 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
Specific Heat Capacity 1.80 J/g-°C
0.430 BTU/lb-°F
Thermal Conductivity 0.175 W/m-K
1.21 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
Unannealed; ASTM Data
Vicat Softening Point 95.6 °C
204 °F
Flammability, UL94 5VA
5VA
UL94 V-0/1.6 mm
5VA

@Thickness 2.50 mm
5VA

@Thickness 0.0984 in
Users viewing this material also viewed the following: